Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

WHAT IS ASME PLATE EQUIVALENT TO DIN 15Mo3

Status
Not open for further replies.

kphjtt

Mechanical
Jul 22, 2005
1
I am badly in need of help. I am trying to find the ASME equivalent for 15Mo3 which I believe is a DIN grade of material. I am looking for the plate equivalent of this material in ASME.

Thanks
 
Replies continue below

Recommended for you

The 15Mo3 appears to be under a DIN material specification (DIN 17175) for carbon/low alloy steel boiler tubes. Here is some information on chemistry and mechanical properties. You can search for an ASME equivalent;

 
Exact equivalent of 15Mo3 is not possible to obtain. However, the nearest ASME equivalent for plates is SA204 (Gr.B is more commonly used).

I would appreciate if you could tell me your application as well. It is because C-1/2 Mo(which is how you would express this material) is hardly being for new constructions. 1 1/4 Cr-1/2 Mo is the preferred choice for substituting an erstwhile C-1/2Mo selection.

Hope you find this information useful.
 