What grade of stainless steel, 303, 304, 316... are operating room hand tools such as a scalpel, laryngoscope blade, or a forceps made of?
 
Replies continue below

Recommended for you

410 grade of stainless steel is more often used for hospital knives etc. These are magnetic in nature but are sharp and strong.
 