Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

What is A610 ?

Status
Not open for further replies.

ramjet005387

Mechanical
Joined
Feb 28, 2002
Messages
2
Location
US
I am looking for information on a metal known as "A610". I found AISI 610 in Stahlschlussel (UNS T20811) listed among high temperature resisting steels. Any help is appreciated.
 
UNS T20811 = H11 tool steel Regards, Wil Taylor
 
UNS T20811 is listed as a Hot-Work Tool Steel (H-11)
AISI grade H-11. Also ASTM A579 Gr. H-11 or A681 Gr H-11.

Hope this helps.
 
it is one of the aluminium casting alloy.you cad search it at metals handbook vol 2
hope this help
 
shapour abd...

I am an ASM member. I looked at the on-line metals desk edition [asm-intl.org site] and could not find reference to any A601 or 601 Aluminum casting alloy. NOTE: by the aluminum designatiomn system A601 would be a "next generation" [improvement of] 601 aluminum alloy.

I request you give me a specific page/location reference for the alloy You cited! Regards, Wil Taylor
 