What type of gate do you recomend? Allmost a pot shaped part 120 x62x11 mm (volume 14cm3 ) has hole (diameter 6 mm ) in center.
Part has uniform thickness 2 mm, material PS. There is one cavity in the injection mold. Gate must be
automatically degated. Diaphragma gate would be suitble but it requires manual degating operation.
 
Replies continue below

Recommended for you

Rauno,

Of course a diaphram gate would be most desirable for this part. It sounds as though your part is too large to try an edge gate. Although you could make a drop down to the center bore (Hole in pot) and have it branch out 3 ways evenly to (3) edge gates.
 
As the answerguy says, except, make the edge gates submarine gates, or cows horn gates for automatic degateing, or put a straight shot directy onto the part, near the edge of the hole, if the gate mark is acceptable. For exact position of gate, it is best to see a model, or at least a drawing. Regards
pat
 
Agree with the comments stated, though you will need a side wall of plastic to sub feed near that hole. If this isn't the case, you might want to consider either a submarine or a winkle gate onto an ejector pin located near the edge of the hole.