Hallo!

What does g1 and g2 represent in EN13445-3 table A-7 figure F4 ?
Could it have something to do with the throat thickness of the fillet welds?

Screenshot_2024-06-27_165345_ybzlmf.png


Thanks!
 
Replies continue below

Recommended for you

consider the side of the triangle.

Regards
 
Ok, so g1 is the throat thickness * √2 ?
 