What designation (AISI or ASTM) does Chromel "A-A" rod belongs?

Status
Not open for further replies.

Saver2008

Mechanical
Oct 14, 2008
112
Hi!

I´m searching for a AISI or ASTM designation for Chromel "A-A" rod or bar with a melting point of 2642°F.

Thank you so much for your help!

 
Replies continue below

Recommended for you

Chromel is pretty much the same as Nichrome V; 80Ni,20 Cr. Try to find ASTM B 82 (it may have been replaced).
 
Indeed, B82 has been replaced (in 1959!) As blacksmith37 notes, Chromel A is 80 Ni-20Cr. The spec you are looking for is ASTM B344. It is for drawn or rolled Ni-Cr-(Fe) alloys.

Aaron Tanzer
 