powerplantcwi
Mechanical
I have a boiler repair that will consist of replacing a section of 2"OD x .201"MW T23 tube with a section of T91 tube. There is a T23/T91 dissimilar weld line just below the repair area and there is no T23 tube stock on-hand but have the T91. I am planning to utilize the NBIC weld method 6 for the T91/T91 weld line and am curious if I can use it for the dissimilar weld as well using the ER80SB8 filler, in place of the recommended CR2WV filler, with the same results to eliminate the need for PWHT of the dissimilar weld in a boiler internal setting. I am aware that I will have to run a separate PQR but would like to know if anyone has done this.