Welding rod to pipe grade application

Status
Not open for further replies.

Jjohnson2020

Industrial
Joined
Apr 2, 2020
Messages
3
Location
US
Hi all, My question is Can e8010 be used with X52 Pipe grade?
 
Yes, but why would you want to. It is ubdertood that most X52 actually meeys X60. E7010 is much used for this application and is somewhat cheaper.
 