Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Welding repairs 100yr old barge?

Status
Not open for further replies.

willard

Automotive
Nov 30, 2002
2
Hi

Having problems welding 10mm plates to bottom of the hull of a 100yr old dutch barge. Using a 376amp 3 phase mig, with 1mm wire, and Ar/Co5% gas.

Problem seems to be linked to corrosion, within the rivetted joint, adjacent to the area where we are trying to weld. This is causing gassing of the weld should we attempt anything other than 50mm backstep technique.

Wonder if anyone has any idea how this problem might be dealt with? Any help much appreciated!

Willard
 