I am reviewing vendor's welding procedures on a Vessel, which requires impact test.
The welding process is SAW. The vendor provided two PQR(s) to support one WPS. Impact test is required. ASME IX is used for the qualification.
PQR-1:
Test coupon thickness: 8 mm
Maximum Interpass temperature 311F;
Maximum Heat input: 68000 J/in
PQR-2:
Test coupon thickness: 19mm
Maximum Interpass temperature: 383F;
Maximum Heat input: 57000 J/in
WPS:
Qualified thickness range: 8-38mm.
My quesions:
(1) Which one is the qualified Maximum interpass temperature: 411F or 483F ?
(2) Which one is the qualified Maximum Heat imput: 57000 or 68000 J/in ?
Please advise. Thicks.
The welding process is SAW. The vendor provided two PQR(s) to support one WPS. Impact test is required. ASME IX is used for the qualification.
PQR-1:
Test coupon thickness: 8 mm
Maximum Interpass temperature 311F;
Maximum Heat input: 68000 J/in
PQR-2:
Test coupon thickness: 19mm
Maximum Interpass temperature: 383F;
Maximum Heat input: 57000 J/in
WPS:
Qualified thickness range: 8-38mm.
My quesions:
(1) Which one is the qualified Maximum interpass temperature: 411F or 483F ?
(2) Which one is the qualified Maximum Heat imput: 57000 or 68000 J/in ?
Please advise. Thicks.