Hello,
i have qualified wps of thickness range 16-50mm with multipule pass. actual pqr on thickness 25mm with impact test , single v groove, i have required 9 pass to fill 25mm thickness, so according to wps thickness range i have to weld 40mm thick but it may required 15 passes .
so increase in number of weld pass with same wps is an essential variable as per asme sec ix and where it is mention in asme plz suggest.
i have qualified wps of thickness range 16-50mm with multipule pass. actual pqr on thickness 25mm with impact test , single v groove, i have required 9 pass to fill 25mm thickness, so according to wps thickness range i have to weld 40mm thick but it may required 15 passes .
so increase in number of weld pass with same wps is an essential variable as per asme sec ix and where it is mention in asme plz suggest.