Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Welding opf MP35N

Status
Not open for further replies.

roozle

Mechanical
Joined
Jun 11, 2001
Messages
28
Location
GB
Can MP35N be welded.?

Also known as: UNS R30035; AMS 5758; Carpenter/Timken Latrobe MP35N.

Thanks,
roozle

Highest Regards,
Roozle
 
Yes, but....
If you are using product in the 'cold worked & aged' condition you will not reach the same mechaical proerties in the welds (or HAZ). Depedning on the service and such you need to be careful where in the process sequence you weld with respect to cold working and heat treatments.

= = = = = = = = = = = = = = = = = = = =
Corrosion, every where, all the time.