Welding on SS formed head

Status
Not open for further replies.

R.Eng

Mechanical
Sep 12, 2019
36
Dear experts,
Are we allowed to do welding on the knuckle region of formed head due to the cracks generated after forming?
The material is SS316L
 
Replies continue below

Recommended for you

Reza.Eng, if the head is to meet some recognized Code or standard I recommend you consult the same. Example: Sec VIII, Div 1, UG-78.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Review some of the more current NBIC's as this case is considered a major repair and the NBIC's may not allow( but I am not sure) repairs in the knuckle of heads.
 
Can you send us more details? (dimensions, photo, etc)

Regards
 
The diameter is about 3000 mm.
Cracks are generated at the outer surface of knuckle region.
Forming has been done at about 350 degree Celsius.
Is it rational to use this range of temp. ?
Do we have any references for this repair?
 
Reza.Eng, give a hint, are you perhaps manufacturing the head? Or something else?

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
snTMan we have formed this head as a top head of column.
 
Then I stand by my first reply.

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 