Welding EN19 to EN24

Status
Not open for further replies.

diptrans

Industrial
Mar 20, 2009
1
Anybody help with the above item? Looking to weld EN19 to EN24 using FCAW what trade name or type of consumable should be chosen and what kind of preheat and post heat need to be applied?
 
Replies continue below

Recommended for you

diptrans;
Based on your post, I would contact the folks below and their technical reps will guide you every step of the way based on your specific application for joining these materials.


Some words of advice;
1. Qualify a weld procedure and your welders
2. Specify some type of post weld nondestructive testing.
 