Hello,
I was wondering if anyone has any information regarding back gouging and when it is required. We have just welded a 3" plate with a backing strip (bevel prep.), removed the backing strip and now are wondering if the side that the backing strip was on should be back gouged and welded?
thanks
I was wondering if anyone has any information regarding back gouging and when it is required. We have just welded a 3" plate with a backing strip (bevel prep.), removed the backing strip and now are wondering if the side that the backing strip was on should be back gouged and welded?
thanks