Is it possible to get a good weld with AR500 (aka Wearalloy 500) to AR500, and AR 500 to A-36 Steel? I have been told that with the carbon content of AR500 at .30 it will be difficult.

Thanks in advance,
Marshall
 
Replies continue below

Recommended for you

AR500 can be readily welded to A-36 with E7018 electrodes with moderate preheat as thickness increases or ambient temperature declines below 50 F.

 