Welding & Brazing Qualification 2

Status
Not open for further replies.

kkg123

Mechanical
Joined
May 12, 2002
Messages
32
Location
IN
how to qualify the person / operator for his work in Welding & Brazing. Are there any test OR codes / standards?
 
There are many cods/Standards for welder performance and procedure qualification.

AWS D1.1 (Structural Welding)
ASME Sec IX
API 1104
Mil Std 248 (Military)
N/S 250-1500 (MIlitary)

And Many others. The actual test will vary depending upon the welding to be performed. Welding Process, Thickness, Diameter for Pipe, backing, Filler metal, backing/shielding gas and many others are typical variables that govern what range a test will qualify a welder for.

The American welding society (AWS) has a standard specification for qualification of welders. See Here
Have a nice day.

G Austin
 
Following are few more relavant standards for welders / welding procedures for metallic materials
BS EN 287
BS EN 288

Hope this helps.

Pras
 
I work for a German steel construction company. I Think we have in Gemany another System for our welding procedure tests compared to the UK. Our WPS do not have to be approved by a special test sample, if the welded steel is not sensitiv in the heat affected zones...in UK you have to do the tests in any case. My question is, if the test- standards acc. to EN 388-3 are completly the same, or is there the possibility to make the tests more easy or have a bigger range of validity for the WPAR, which are the approved institutions for the WPAR in UK?
Thanks for any information
 
Please let me know which is the best specification for Brazing & Welding Qualification. Our application is Compressor Manufacturing.
Following is the list all have supplied :
1.AWS D1.1 (Structural Welding)
2.ASME Sec IX
3.API 1104
4.Mil Std 248 (Military)
5.N/S 250-1500 (MIlitary)
6.BS EN 287
7.BS EN 288
8.Brazing. Brazer approval BS EN 13133:2000
9.Brazing. Procedure approval BS EN 13134:2000
 