Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

welding aluminum

Status
Not open for further replies.

doorsRus

New member
Joined
Oct 10, 2001
Messages
5
Location
US
This is the problem I have. I need the advice of experienced engineer or welder.
I have a project to build a aluminum door for an aircraft. It is an airstair door. Approx. 4 ft by 5 ft. It is made up of many sheetmetal parts all 6061. All the same thickness .063. Some parts will be bent to shape on a brake. Others will be cold formed to shape using a shrinker stretcher. All the parts will then be put in a jig fixture for welding, which will result in essentially a shell. The problem that a previous manufacturer had was warping.
I saw at one time a welder first tacking together, than welding little sections (approx 1 inch) at time at opposing locations. I think it was for allowing even heating of the aluminum. I would think with the addition of "clamping until cooling" that this might reduce the warpage.
Is this correct?
Karl
 
Post your quiry to the welding foram. They will be able to tell you what the weld will do to the metal.
 