AUSTIN316L
Industrial
Hi
We've welded 316L base metal with 308L filler (by mistake). I would like to know of any negative effects if the product is used in a potable water application, no more than room temp, static load (in the region of 20 ksi).
The product will be passivated prior to use.
We've welded 316L base metal with 308L filler (by mistake). I would like to know of any negative effects if the product is used in a potable water application, no more than room temp, static load (in the region of 20 ksi).
The product will be passivated prior to use.