Welder qualification for ASME Section IX and API 1104 have different requirements and do not overlap. Further, you cannot use an ASME WPS to qualify welders to API 1104, and vice versa.
Functionally, from a welding perspective, there will be little difference, but from a compliance perspective, welders need to be qualified to the code of construction using welding procedures qualified to that same code of construction.