Mar 18, 2013 #1 anasbabu Materials Joined Mar 18, 2013 Messages 1 Location SA Please help me. I have one welder maximum allowed thickness 10mm and another welder have maximum allowed 11mm. CAN I ALLOW these welders do 21mm thickness total weld. First welder up to 10mm remaining other welder.please refer a code with para
Please help me. I have one welder maximum allowed thickness 10mm and another welder have maximum allowed 11mm. CAN I ALLOW these welders do 21mm thickness total weld. First welder up to 10mm remaining other welder.please refer a code with para
Mar 18, 2013 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Yes, provided the welders are qualified and you have a qualified WPS. Review QW-250, and QW-306. Upvote 0 Downvote