I am reviewing a structure designed in 1967 and have come across welded wire fabric designated as “ 66 – 55 W.W.F.”. I have not seen this designation before. Does anyone know the properties As/ft of this designation?
 
Replies continue below

Recommended for you

This means number 5 gague wire at 6 inches on center.
 
Add to my previous answer "each way".
 