Weldability Range, What does this value mean?

Status
Not open for further replies.

winter39

Mechanical
Sep 20, 2004
6
I curently have a material specification sheet that has some parameters for Resistnace Spot Welding USIBOR 1500P material. It states the minimum current (12.3 kA), maximum current (13.7 kA) and weldability range (1.9 kA). What does the weldability range value mean?
 
Replies continue below

Recommended for you

Does anyone have any insight on the term "weldability range"?
Thanks
 
winter39;
Did some research on this, and the closest match I could find in resistance welding terminology is a brochure on a Miller Aerowave Hybrid AC/DC Constant Current Squarewave Arc Welding Power Source. In their description, they refer to Welding Amperage Range. In the context of weldability, this may be the same definition used by another manufacturer. Weldability refers to the ability to produce a sound weld deposit.
 