Dec 27, 2006 #1 MatEngTED Materials Joined Sep 27, 2004 Messages 24 Location US Need to know what weld wire to use for AMS # 4214H, UNS # AO3550, Alloy 355.0-T6 Aluminum Casting. Please advise. Thanks.
Need to know what weld wire to use for AMS # 4214H, UNS # AO3550, Alloy 355.0-T6 Aluminum Casting. Please advise. Thanks.
Dec 27, 2006 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Go the web site below and contact these folks; http://www.alcotec.com/default.html Upvote 0 Downvote