Would like to know how to calculate width and length of welds. My gap between metals is between 1/16 and 1/8 in aluminum. Please advise. Thank you in advance for your information

Stephen
LnTxn@aol.com

 
Replies continue below

Recommended for you

What is your weld profile? Fillet? Butt?
 
That would be a fillet weld

Stephen