templetonc
Aerospace
I would like to weld two 1/8 fillet welds 1/4 inch long on 1” rod 180° apart. Which is the proper way to callout the weld per AMS 2.4:
1/8 (Fillet Symbol) 1/4”-180°
or:
1/8 (Fillet Symbol) 1/4”-1/2”
or:
1/8 (Fillet Symbol) 1/4”-2 23/64”
NOTE: 2 23/6 is the approximate circular distance around the perimeter of the rod.
1/8 (Fillet Symbol) 1/4”-180°
or:
1/8 (Fillet Symbol) 1/4”-1/2”
or:
1/8 (Fillet Symbol) 1/4”-2 23/64”
NOTE: 2 23/6 is the approximate circular distance around the perimeter of the rod.