I propose to use a 4-40 UNC weld stud as a replacement for a length of studding in a tapped hole. Although the weld stud principle is well documented, I haven't yet found a definitive answer to this question:
Is it only the fused pip of the stud which provides the strength or does the welded area extend across the whole face of the stud? I suspect the former is true and that the weld witness seen around the periphery of the stud face is not actually adherent and doesn't add to the strength of the joint.
Any ideas please? Many Thanks.
Jim
Is it only the fused pip of the stud which provides the strength or does the welded area extend across the whole face of the stud? I suspect the former is true and that the weld witness seen around the periphery of the stud face is not actually adherent and doesn't add to the strength of the joint.
Any ideas please? Many Thanks.