Some design codes define a min distance between welds as a good engineering practice, such as PD5500.
In a lot of cases, nozzles and attachments can sometimes be so near to a main weld seam (and in my present case on it).
Does anybody have any thoughts about this matter?
If like in my particular case where no changes to the construction is acceptable, is there anything that one can do to satisfy ones concerns?
Many thanks in advance