BlackwellS
Mechanical
Gents,
I have a reduced crude vacuum transfer line (700F) subject to localized napthenic acid attack. Metallurgy on the line is 5CR (A335 GR P5). One of our options is to upgrade a number of small-bore connections (thermowells, vents, etc.) and L.R. ells to 317L. Could someone provide general guidance on welding 5CR to 317L? Is this dissimilar weld even possible? Is there a single rod available, or would we need to lay down intermediate passes of varying weld metal? I assume PWHT would also be required.
Also, could anyone recommend a good welding "handbook," or guide? Maybe from the WRC or AWS that may assist? Thanks!
I have a reduced crude vacuum transfer line (700F) subject to localized napthenic acid attack. Metallurgy on the line is 5CR (A335 GR P5). One of our options is to upgrade a number of small-bore connections (thermowells, vents, etc.) and L.R. ells to 317L. Could someone provide general guidance on welding 5CR to 317L? Is this dissimilar weld even possible? Is there a single rod available, or would we need to lay down intermediate passes of varying weld metal? I assume PWHT would also be required.
Also, could anyone recommend a good welding "handbook," or guide? Maybe from the WRC or AWS that may assist? Thanks!