Hello Gents,

I am newer to Welding. I was going through AWS D1.1 & D1.8 to check the values and ranges for:
1. "Weld Deposition Rate" for SMAW & FCAW.
2. Weld Single pass thickness for SMAW & FCAW processes

As-usually I checked it in several clauses but due to lack of knowledge to AWS codes I am unable to find it. Is there any body to help out me to solve these tiny mysteries.

Cheers

A. Ahmed

 
Replies continue below

Recommended for you

not sure about d1.8. But for d1.1 single pass thickness maximums are in table 3.7. Deposition rates aren't limited under d1.1. I would think that's because deposition volume is a function of amperage and technique. It would be difficult to quantify maximums or minimums.
 