I can't find any default weight values for Carbon & Alloy Steel Solid Wire 706s6 SuperArc L-56
MIG wire per foot or meter or inch.....

In order to complete an EIQ I need a MHDR in 1000 lbs/hr units on a welder. I have an MHDR in
m/min--but can't find a weight per length for the wire.
 
Replies continue below

Recommended for you

The density is the same as carbon steel in any other form. I use .2833 for the weld costing application I use.

However depending on the transfer mode, not all of this metal is deposited in the weld. The deposition rates are usually available from the manufacturer for many processes.