I would like to receive comments of the experienced one. I am working on a paper plant project and for reject lines, overlay material will be selected for wear resistance.
What is your suggestion for stellite or tungsten carbide?
Are there any specific parameters to compare like hardness etc?
Pls. advice. Thanks in advance.
 
Not any exceesive condition for heat and pressure. There are many different lines with similar conditions. Not above 150 psi.
 