WCB refers to a Grade of cast carbon steel in ASTM/ASME A/SA-216, which is "Specification for Steel Castings, Carbon, Suitable for Fusion Welding for High-Temperature Service". Grades of carbon steel castings are identified as WCA, WCB or WCC and vary based on alloy content, and mechanical properties.