dears I want to share you a problem that we face in our pipeline.
that we receive a high amount of wax in terminal during pigging specially during pigging operation and some times it lead to blockage in terminal control valves and accumulated wax in bottom of tanks.
the pipeline is 28" OD 1500 km transfer crude oil from main fields and two injection points .
now the main suspected causes are. the crude characteristics , combined with the laminar flow and the terrain change.
this in short
please if you experienced such problem like that share your ideas and how you solve that.
Regards
that we receive a high amount of wax in terminal during pigging specially during pigging operation and some times it lead to blockage in terminal control valves and accumulated wax in bottom of tanks.
the pipeline is 28" OD 1500 km transfer crude oil from main fields and two injection points .
now the main suspected causes are. the crude characteristics , combined with the laminar flow and the terrain change.
this in short
please if you experienced such problem like that share your ideas and how you solve that.
Regards