Quiron

Industrial
Nov 25, 2013
3
Hello all , I´m new on the forum so please excuse me if I go past any protocol.

We have a Trumpf Tc6000l with a 2kw LASER . Over the past 11 years we had 3 water leaks in our resonator , the last leading a complete resonator change .All maintenance is done in accordance to the manual and the demineralized water is certified .
Is this normal ? If not , any ideas on what is going wrong please .

Thank you in advance.

Quiron
 
Replies continue below

Recommended for you

This was there report :

"The development of corrosion is depending on different factors and can occur after 1000h or 10.000h e.g.

- The admixture in the cooling water to avoid corrosion was not sufficient

- Missing maintenance on the resonator

- …."

The admixture was added in quantities and timing as specified in the maintenance manual.

After cutting one of the faulty cooling coils, no corrosion was found ,only a very small pierced like hole.

 