Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Water composition for hydrotest

Status
Not open for further replies.

andygo11

Materials
Joined
Feb 15, 2013
Messages
20
Location
CA
Hi, I have a question regarding the hydrotest water. Is there any codes or practice we can follow in terms of the water used for hydrotest? How to prevent the potential corrosion issue? Thanks.
 
Have you searched eng-tips? This has been discussed a number of times before.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
50 microns seems to be a rule of thumb for maximum acceptable particle size for hydro test water (at least for carbon steel). I have researched unsuccessfully (including Eng-Tips) the technical basis for this magic number. Does anyone know where the 50 microns come from? ... your feedback is much appreciated.
 
Don't know the answer but the smallest sand size is approximately 50 microns.
 
Dear Andy,

Refer DEP 31.40.40.38-Gen.


DHURJATI SEN
 
Dhurjati, DEP 31.40.40.38 seems to be a Shell document. Do you know how I can get it?; I searched the Internet for a download site and could not find any.

Regards, Alberto Valdes
 
Dear Alberto,

Shell DEPs are not available for free. You (your company) need to buy it.

Regards.

DHURJATI SEN
 