Dear all,

Currently I am doing some research on dipped product using water-based chlorosulfonated polyethylene (CSM).
We are facing severe crack body and low tensile in my research.

I would like to ask is there any typical formulations for CSM to achieve tensile min 18MPa and can eliminate the crack body?


 