We are using Alloy Steel Bolts BS 1506-621 A
Carbon Steel Nuts BS 1506-162, what would be the specification for the washers.
 
With no other information, I would go to the bolt and nut specifications and see if they state what they are to be used with. It's been a while, but seems like the A325 and A307 specs spell this out pretty clearly, so perhaps the referenced specifications do as well.
 