May 26, 2011 #1 zebmahar Materials Joined Dec 12, 2010 Messages 46 Location SA It would be very appreciated if some one tells me the name and web address of well known laboratory having a capability to perform Hydrogen Induced Cracking (HIC) & Sulfide Stress Cracking (SSC) Tests. Thanks Zebmahar
It would be very appreciated if some one tells me the name and web address of well known laboratory having a capability to perform Hydrogen Induced Cracking (HIC) & Sulfide Stress Cracking (SSC) Tests. Thanks Zebmahar
May 27, 2011 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US I would give these people a call. As far I know now they perform about any test around and do it right. http://www.exova.com/ Upvote 0 Downvote
I would give these people a call. As far I know now they perform about any test around and do it right. http://www.exova.com/
May 27, 2011 #3 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US Omni Metals Lab in Ann Arbor, MI (USA) routinely performs HIC and SSC testing according to NACE requirements. http://www.omnimetalslab.com/ Another lab that frequently performs this type of testing is Stork Testing & Metallurgical Consulting in Houston, TX. http://www.storksmt.com/Stork/21173/Sour_Service_Corrosion_Testing.html Exova also offers these services. Upvote 0 Downvote
Omni Metals Lab in Ann Arbor, MI (USA) routinely performs HIC and SSC testing according to NACE requirements. http://www.omnimetalslab.com/ Another lab that frequently performs this type of testing is Stork Testing & Metallurgical Consulting in Houston, TX. http://www.storksmt.com/Stork/21173/Sour_Service_Corrosion_Testing.html Exova also offers these services.