Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Vickers hardness database for steels?

Status
Not open for further replies.

aniiie

Materials
Jul 5, 2005
5
HI, I would like to ask, if anybody knows whether any database of material hardness (Vickers HV20 particularly) exist. In the norm describing the testing procedure is not given any information about this. Construction steel (TS = 450-650MPa)is the main focus. Thanks a lot. Nice day!
 
Replies continue below

Recommended for you

aniiie;
Basically what you are asking is the following, what is the acceptable range of hardness for construction steels having an ultimate tensile strength range of 450-650 MPa.

Try searching the internet for hardness to ultimate tensile strength conversion for steels.
 
ISO 18265 is the international reference for converting hardness and tensile strength. You can obtain it directly from ISO or one of its distributors.
 