venturi air cleaners

Status
Not open for further replies.

3800sc

Mechanical
Jul 14, 2010
8
does anyone know of a company that sells venturi air cleaners. I am dealing with a process that has a vacuum line connected to a large conical tumble dryer to dry nylon.

The problem is a monomer is released from the nylon and clogs up the vacuum system causing downtime.....i am thinking a venturi air cleaner with a cool chamber to make the monomer fall out of the stream may work.

any suggestions are greatly appreciated as im having no luck with web searches
 