Ive been asked to get a 42% FVF in a fibreglass / polyester part using VARTM, measuring about 3mm thick.What's mad is that chopped strand has been requested in there also, so not a hope 40% FVF is going to happen.
Im proposing doing a layered biaxial or multi-axial lay-up with the finest CSM mesh I can find! Does that seem reasonable or have I just been looking at this too long and am missing the bigger picture?!?
Thanks dudes