Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Vapor fraction and H2S partial pressure

Status
Not open for further replies.

CoCoE

Petroleum
Joined
Mar 9, 2012
Messages
118
Location
JP
I would like to seek the opinions on below things.

In a slug catcher,

Top: Gas line (with H2S partial pressure approx 15 psi, CO2 approx 25 psi)
Bottom: Sour water (Zero vapor fraction, 99.8% water, 0.02% H2S+CO2)

In such a condition, for selecting the material for the bottom piping, how to consider H2S partial pressure? I feel that I must consider the Top gas piping process parameters as equilibrium gas phase. But some people conflict this by saying as there is no vapor fraction, pH2S is very very low, and this is completely in aqueous phase.

What is the correct method?

Kristy
 
Refer to C.2 of ISO 15156-2, particularly the NOTE under list item a)

Steve Jones
Corrosion Management Consultant