Good day,
I am looking for some of expert opinion Re: Valve type and material (if possible) to be used in Catalyst Cracker unit.
General process condition are (Apology I am not a Process Engineer):
a. Catalyst used is some kind of sand blasting powder look alike
b. Catalyst along with other mixture velocity on 10" pipeline is approx 25,000 liter/minute. Highest process temperature is 450 deg Celcius, especially during mixing process.
At some point of the pipeline and valve, it is eroding the inner surface (due to turbulence, high velocity, powder containment)
c. For throttling purpose we use 10"-300# Gate valve Body: ALLOY STEEL 5Cr-0.5Mo; Trim in general is AISI 316/STELLITE 6.
d. Every 6 months to 2 years, valve used for throttling found to have either disintegrated trim and or even some hole in the valve body (located below the bonnet).
Highly appreciate shall anyone could provide their insights for material (body and trim) and valve selection for this kind of services.
Regards,
MR,
Valve Engineer in one of Pernis Complex Refinery
I am looking for some of expert opinion Re: Valve type and material (if possible) to be used in Catalyst Cracker unit.
General process condition are (Apology I am not a Process Engineer):
a. Catalyst used is some kind of sand blasting powder look alike
b. Catalyst along with other mixture velocity on 10" pipeline is approx 25,000 liter/minute. Highest process temperature is 450 deg Celcius, especially during mixing process.
At some point of the pipeline and valve, it is eroding the inner surface (due to turbulence, high velocity, powder containment)
c. For throttling purpose we use 10"-300# Gate valve Body: ALLOY STEEL 5Cr-0.5Mo; Trim in general is AISI 316/STELLITE 6.
d. Every 6 months to 2 years, valve used for throttling found to have either disintegrated trim and or even some hole in the valve body (located below the bonnet).
Highly appreciate shall anyone could provide their insights for material (body and trim) and valve selection for this kind of services.
Regards,
MR,
Valve Engineer in one of Pernis Complex Refinery