Hi all! Is trim 1 applied on gate valves for steam tracing manifolds (3.5k steam) the right selection?
 
Replies continue below

Recommended for you

For the most part Trim 1 is not usually in standard valves anymore. From my experience the only people using Trim 1 are nuclear power plants trying to reduce Cobalt in the system.

Trim 8 is used on most class 150 through 600 valves and Trim 5 for class 900 and above.
 