Valve Seat Hardness

Status
Not open for further replies.

Joesteam

Chemical
Joined
Dec 23, 2002
Messages
139
I am not very knowlegable in this area, so please be kind.

I am working with specifying engineers and they have a grandfathered specification for stellited valve plugs and seats for 200 psig steam service (district steam = dirty & wet) as an overlay on 316 SS material.

I have a valve with hardened 416 SS material that the manufacturer says is plenty hard and robust for this application.

I am thinking maybe that the stellite is a bit harder, however since it is just a overlay there may be problems with this in the long run. I would like to have the engineer at least allow the hardened 416, it would save the customers money and lead time.

Any ideas??
 
For many applications, 400 series stainless is sufficient and has been a standard offering for many valve manufacturers. Is the 416SS hardened through a nitriding process? If so, once that finite layer wears through, what can be done to repair the valve?

I2I
 
I believe the 416 is heat treated for hardness, the manufacturer data says 'hardened to 38 HRC' where an alternate trim is 316SS with CrCo-A hardfacing alloy.
 
N08367, Alloy 6, B 688 is commonly used for errosive applications. Some manufacturers avoid the trade name such as Stellite, Haynes, Stoody Deloro, etc. Deloro Stellite covers a family of alloys.
 