Hi,
i am looking for a spiral wound gasket or an alternative gasket to seal a valve body joint, pressure class 2500.
Problem with spiral wound gaskets e.g. "Flexitallic" or others are all limited to around 6000psi (420bar) which is the CL2500 operating Rating at ambient temp.
BUT you need to test the vale in Advance up to 1,5x nominal pressure which is around 9000psi (630bar) .
We had leakage in the past here.
Or does anybody know an inexpensive alternative sealing option?
Conditions:
up to 9000 psi (630bar) at ambient temp.
up to 840°F (450°C) op. temp. according CL2500 Rating
Thanks!
i am looking for a spiral wound gasket or an alternative gasket to seal a valve body joint, pressure class 2500.
Problem with spiral wound gaskets e.g. "Flexitallic" or others are all limited to around 6000psi (420bar) which is the CL2500 operating Rating at ambient temp.
BUT you need to test the vale in Advance up to 1,5x nominal pressure which is around 9000psi (630bar) .
We had leakage in the past here.
Or does anybody know an inexpensive alternative sealing option?
Conditions:
up to 9000 psi (630bar) at ambient temp.
up to 840°F (450°C) op. temp. according CL2500 Rating