Can you calculate the sheet area you need by working out the surface area of the mold? How much does a plastic sheet thin out when it sags?

I am building a vacuum forming machine for a prototype and need to estimate the forming area/frame size needed.

Thanks
 
Replies continue below

Recommended for you

The ratio of straight shape to curved shape will point to the amount of thinning. The heater temp should be below melt temp. Use a generous corner radius, about 3 x t, at the flat to curved transition.
 