I'm developing a tolerance block for various commodities for my company. I've researched and met with suppliers to review our final format tolerance blocks.
In regards to Vacuum forming, does anyone have an angle tolerance recommendation? Machining, sheet metal and compression molding are pretty well defined and available.
I also have general tolerances for the standard angles for draft.
For example 3-5 degrees, 5 degrees whenever possible. But the tolerance for those angles are not defined.
Any input would be appreciated.
In regards to Vacuum forming, does anyone have an angle tolerance recommendation? Machining, sheet metal and compression molding are pretty well defined and available.
I also have general tolerances for the standard angles for draft.
For example 3-5 degrees, 5 degrees whenever possible. But the tolerance for those angles are not defined.
Any input would be appreciated.