the customer is saying that he will weld A106 Gr B to A105 pipes
but he only have a qualified weld procedures for 52 ksi and 65 ksi
he is asking if he can do that? or need to change the material ?
but he only have a qualified weld procedures for 52 ksi and 65 ksi
he is asking if he can do that? or need to change the material ?